Initial washing for ITO Patterning & heat treatment after Photo-resist coating
|




 |
Selective exposure after P/R coating, developing, ITO etching, and P/R peel-off to form a desirable ITO pattern
|




 |
Applying insulation layer evenly on the surface whose ITO Pattern is formed in order to prevent Short of upper/lower substrates caused by conductive corpuscles
|




 |
Applying Alignment substance on the ITO Pattern or Insulation Layer for better alignment property, and forming alignment layer to have a certain direction of alignment
|




 |
Pressing Sealant between Segment Panel and Common Panel so that LC can be injected in that area
|




 |
Assembling Common Panel on which Spacer is spread and Segment Panel on which Sealant is pressed within the area of Align Mark, and hardening it at high temperature and high pressure so that Cell Gap needed can be formed
|




 |
Scribing LCD Panel into a stick shape to inject LC
|




 |
Injecting LC into the inner Cell by vacuum method
|




 |
Sealing LC inside the Cell and making the Gap even by using Press, and sealing the injection port
|




 |
Scribing Sticks with a scriber into the unit of a Cell
|




|
Supplying electrical signals to Cells to drive, and checking disconnection, short, driving voltage difference, and contrast condition, etc
|




 |
Attaching plates which have polarizing effect (transmitting light vibrating at the perpendicular direction only) at the top & bottom of the scribed cells
|

|
 |
|